RadiatorsandCorrugated Cooler wallis the normal Transformer Cooler Part used to cool the transformer oil.
JTFY Corrugated Fins Wallalso named Corrugated Cooling Wall or corrugated transformer tank cooler ,it is one part of distribution transformer tank body.
welded corrugated finwall by JTFY auto fins wall seam welding machine
JTFY has Fully Automatic Corrugated Fin Walls pressing/folding/forming and welding machines for distribution transformers cooler(corrugated fin wall), with all the state of the art technologies.
We can manufacture corrugated walls with different profile, with spot welding, with strip.
Following the indications on the customer’s drawings, all kinds of bending may be carried out, on either side of the wall or on the whole wall, so that the tank construction may be completed with only one weld.
3.Corrugated FinsTransformer CoolerWall with Embossing:
Single Embossing & Double Embossing:
Corrugated Fins Wall with single & double Embossing
Bottom Embossing:
corrugated fin wall with embossing
Transformer Cooler – Corrugated Fins Walls technical details:
JTYF Fins Walls are manufactured with SPCC STEEL SHEET material height range from 400mm up to 1600mm, with thickness of 0,8mm – 1,0mm – 1,2mm – 1,5mm and with a depth of the fins from a minimum of 40mm to a maximum of 400mm.
On the Fins we could apply both embarrassments, to make stronger the fin wall, than spot welding, in order to grant an higher oil pressure resistance of the entire tank.
JTFY can manufacture also corrugated walls with full automatic. A better configuration of the space inside the fins in order to make the oil circulate better, helping the whole heat dissipation of the tank.
On the corrugated walls JTFY can apply a metallic strip that help the welder during assembling operations and welding processes, giving to him a perfect straight shape to handle and a strength edge resistance.
In the end JTFY can perform bending on the edge sides of the corrugated wall or bend directly in the middle of the fin wall that may be an half tank, saving time during welding operations.
Transformer Cooler-Corrugated Fins WallsEmbossing:
Now JTFY can produce Single, Double,Bottom Embossing Corrugated Fins Wall.The embossing has been designed to make the corrugated walls more stronger, especially in the big tanks where the pressure of the oil is huge and where the depth of the fins is high.
When design machine parts / prototypes by 2D engineering method, we can adopt simplified drawing method: 1.When the object ( mechanical part ) has several identical structures (teeth, slots, etc.) and distributes according to certain rules, only a few complete structures need to be drawn. The rest are connected by fine lines, and the total number of structures is indicated. Mechanical part Examples of Simplified Drawing of Mechanical Drawings : Examples of Simplified Drawing of Mechanical Drawings for Same Structure and Simplified Drawing Same Structure and Simplified Drawing 2.A number of holes with the same diameter and regular distribution (round holes, screw holes, sinks, etc.) can be drawn only one or several, the rest can only be represented by the center line, and the total number of holes should be indicated when the size of holes is marked in the figure. Simplified Drawing Method for Regularly Distributed Holes Simplified Drawing ...
After the first metal part be tapped, we always to check it: if pass the thread gauge inspection? The inspection result is OK, we can do mass production. If it fails, We should consider which reasons cause tapping faiulre. KYLT provide Metal Machining services for: WEDM, EDM, DRILL, TAPPING , CNC LATHING , CNC MILLING , ALUMINUM / MAGNESIUM / PLASTIC RAPID PROTOTYPES MAKING . 1PCS ORDER IS ALLOWED. Aluminum CNC machined workpiece Normally, the following reasons may cause screw thread faiulre: 1) UNQUALIFIED TAP Tap is wear or bad 2) QUALIFIED DRILLING HOLE (BEFORE TAPPING) If the hole is too small, because of friction, will increase the difficulty of tapping, while tapping faster wear, and vice versa, the hole is too big, it can easily tap into, but the quality of teeth is very poor, because the diameter of teeth will become larger, relative to the screw nut bonding force is insufficient, easy to slide teeth. In M3 *0.5, the correct hole (general i...
CNC milling process adopt Down milling or Up milling ? Which milling method is better? Down Milling & Up Milling Definition Down milling: refers to the cutting speed direction of the cutter is the same as the moving direction of the workpiece. Up milling : refers to the direction of cutting speed opposite to the direction of movement of the workpiece. CNC milling work, How to distinguish Down Milling and Up Milling. WHEN MILLING WORKPIECE OUTLINE: Clockwise feeding and programming along the outline of the workpiece is Down milling. Counterclockwise programming and feeding along the outline of the workpiece is Up milling. WHEN MILLING THE INNER CONTOUR OF THE WORKPIECE: Clockwise feeding and programming along the inner contour of the workpiece is downmilling. Counterclockwise programming and feeding along the inner contour of the workpiece is reverse milling. CNC UP & DOWN MILLING CHARACTERISTICS OF DOWN MILLING AND UP MILLI...
评论
发表评论